i shot it over white and it looked good .
silver it was deep. and silver met
Announcement
Collapse
No announcement yet.
Transparent red over what???
Collapse
X
-
Guest replied
-
Try red for a base coat. I did a custom MC frame, fenders and tank with candy (translucent) metallic (gold flakes) red over a base of red metallic with silver flakes. Looked awesome.
Leo
Leave a comment:
-
Re: Transparent red over what
Hey 1Timber:
Most trans colors need a chrome or alum base color.
Good Luck
Bob
Leave a comment:
-
Transparent red over what???
I am coating a small rail in transparent red with added metalic any recomendations for an undercoat I want a deep look the tubing is cromemolly and mild steel??Tags: None
Leave a comment: