Oven - Here is my custom build...

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • transam
    replied
    Originally posted by kchotboat
    Originally posted by transam
    here you can see more pictures...

    if you need some info just ask.

    http://fbody.ca/ovenpowercoating.html
    I like your spray booth also. I made mine to large and takes up to much space in the garage.
    What did you use to insulate the oven with?
    My spray both are just the good size yes & got all paint back, no lost, almost the same size as the oven... Since it useless to have someting more bigger than the oven i use..

    insulation are plain 6" construction fiberglass for home, just make sure to take the one whitout any "paper sided".

    Leave a comment:


  • kchotboat
    replied
    Originally posted by transam
    here you can see more pictures...

    if you need some info just ask.

    http://fbody.ca/ovenpowercoating.html
    I like your spray booth also. I made mine to large and takes up to much space in the garage.
    What did you use to insulate the oven with?

    Leave a comment:


  • transam
    replied
    here you can see more pictures...

    if you need some info just ask.

    http://fbody.ca/ovenpowercoating.html

    Leave a comment:


  • transam
    replied
    Its not finished nicely (my top/side sheet metal was done quickly) but work well, heat very quickly too.

    I will take some detailed pictures whit more info since it apear some interest.. Let me some time.. i will be back whit more info.

    Leave a comment:


  • Popeye
    replied
    I agree, it looks great.
    Does it work as good as it looks?

    Leave a comment:


  • kchotboat
    replied
    looks good. Can you post more info on the construction of it.

    Leave a comment:


  • transam
    started a topic Oven - Here is my custom build...

    Oven - Here is my custom build...

    Here is my Oven ,

    Cost 550$ ca. 23 x 23 x 5'f

    Insulated 6", Build whit an older home oven (element, controler, fuse rack, temp sensor) & an older fan i got for free at my near electrical shop..