the hose holds 5lbs .. but i shoot from 8-10 depending on the powder i am shooting ....
Tip: use a moister filter.. and replace then 1 or more times a month.
Announcement
Collapse
No announcement yet.
Gun Pressure?
Collapse
X
-
Guest replied
-
Re: Gun Pressure
I set my air pressure at 15psi when I pull the trigger it drops to roughly 10 psi.
Works well.
Bob
Leave a comment:
-
8 to 10 # is normal , I adjust my regulator on the gun as needed..some times more, some times less...and if I get really frustrated i put it in hurricane mode....
Leave a comment:
-
Gun Pressure?
Hello all, Can anyone tell me what pressure to set the gun at for coating? Are there different settings for certain objects and materials? Thanks all!Tags: None
Leave a comment: