    OK I had a Rush Job, only becuase I had too much planned and took on a single Piece job. It was a dogbone for a Fiero. Well I put it in the oven to out-gas and got set up. Out-gas time was up so I hung on the peg in the booth and Stated dusting it. Man it was still hot!!!! And the powder flowed right away and stuck like crazy! First time I dusted something that was still hot and what a difference it makes!!!! I never got Coverage like that before. Im going to start dusting hot now!!