    replied
    Yea, whenever I get some spare money around, I think I'll give that temp gauge a try.

    Leave a comment:


  • customandsound
    Guest replied
    it look like a good 1 but the cable i would be worried about i got a martha steward one at k marts i am not sure if caswell sell's one like that i will check ...

    Leave a comment:


  • wamontgomery
    replied
    Chuck, I was searching ebay, this looks like it would be a good probe temp gauge.....

    http://cgi.ebay.com/ws/eBayISAPI.dll...MakeTrack=true

    Leave a comment:


  • wamontgomery
    replied
    Originally posted by customandsound
    i got a lcd one that is for the house oven... i know first hand how quick that little box will dry out your eyes.... let me find a link i will post it .. you can get one from ebay for under 30 bucks
    That'd be great Chuck, thanks!

    Leave a comment:


  • customandsound
    Guest replied
    Looks good ... i need to blow the dust off the part i have and put a pic up then ebay it ...

    Leave a comment:


  • customandsound
    Guest replied
    i got a lcd one that is for the house oven... i know first hand how quick that little box will dry out your eyes.... let me find a link i will post it .. you can get one from ebay for under 30 bucks

    Leave a comment:


  • wamontgomery
    replied
    Here's the top plate I did! I went for the brushed aluminum look on top and put red in the engraved letters, the brushed aluminum looks kinda uneven in the pics, but it's awesome in person!

    http://www.joehoskins.com/Uploader/U...op%20plate.jpg

    Leave a comment:


  • wamontgomery
    replied
    Ok will do. One thing I need is some kind of temp gauge that has a little probe end on it. I have one of those infared temp gauges and I put it up to a little crack that is open and shine it down on the part, well the heat coming out melted the head of the temp gauge. Any idea on what temp gauge has a probe on it that I can drill a hole and stick it inside the oven and keep the gauge part outside the oven?

    Leave a comment:


  • customandsound
    Guest replied
    your welcome ... I am glad it worked for you.. I will be refining some stuff here so keep a eye out in the sticky section for them...

    Leave a comment:


  • wamontgomery
    replied
    Yep, and I put insulation on the sides and top. It works good. Thanks Chuck.

    Leave a comment:


  • customandsound
    Guest replied
    look's good .. did you use the oven set up i talked about? the funny part is i got a top plate the same cover for that intake ... It never made it on my car..

    Leave a comment:


  • wamontgomery
    started a topic Upper intake I did SUPER Mirror red.....

    Upper intake I did SUPER Mirror red.....

    Well I was busy today prepping and cleaning this upper intake to hurry up and get it powdercoated. It's off of a 5.0 HO off my stang, I still need to clean up the top plate and do that in a nice color sheme. I did it in a super mirror red, I think it turned out pretty good. I finally got it so my oven get's up to temp easily now, and stays right around where I need it. Anyways, here are the pics.


Working...
X