Announcement

Collapse
No announcement yet.

Glow in the Dark Additive Help HELP!!!

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Blademan
    replied
    Re: Glow in the Dark Additive Help HELP!!!

    I've gone as far to apply the powder under ulra violet light, makes me rember the 60's again............

    Leave a comment:


  • jtagger19
    replied
    Re: Glow in the Dark Additive Help HELP!!!

    glow over black won't glow as good , it will glow but not as good as light colors
    I have use it over red and blue and it still works nice.
    ussing it over polish aluminum works, it will dull the finish a little but works nice.

    I buy the glow additive and mix it with 1-1/2 Lb of clear powder
    just add it and shake it.

    BTW charge the powder and coat at a low light so you can see what you are doing and get an even coating , the biggest problem I've had with glow in the dark clear is that if you don't get a perfect even coat it will glow more in some spots .

    Leave a comment:


  • Netnut
    replied
    Re: Glow in the Dark Additive Help HELP!!!

    I used an empty 1 gallon ice cream container, put my clear coat in, then the holographic pigment, then used an electric kichen mixer (bought from the trift store Can$ 5.00) and mixed for about 5-8 minutes
    Hope this helps

    fr

    Leave a comment:


  • hoytheld
    started a topic Glow in the Dark Additive Help HELP!!!

    Glow in the Dark Additive Help HELP!!!

    Can I coat something in Gloss Black...then go over with the glow in the dark added to gloss clear?

    Or..if I polish a stainless steel item and coat it with the glow added to gloss clear...will it still look glossy..or will it dull it down? give it a green hue??

    Also, what is the best way to mix the additive with the powder....add it and shake the dog **** out of it??

    thanks
    jason
    Last edited by hoytheld; 08-27-2005, 12:43 AM.
Working...
X