This has been happening for the last couple of weeks, and it's really ****ing me off now.
While spraying, the powder comming through the gunn will slowly diminish. Then I('ll shake the gun (while still spraying) and then more will flow out, and then slowly diminish; the process repeats. Sometime without shaking it, the gun spits out a big cloud of powder. it seems the best wayt o keep a consistant stream is to continually shake the gun while spraying, but that gets tiring very quickly.
I only fill the cup up about 1/3 of the way, I have constant air at about 8 psi. I have 2 water seperators plus the water trap on the gun. I do live in a fairly humid climate. I shake the powder and check for clumps before attaching the cup to the gun. I have taken the gun apart to clean it to keep the trigger from sticking, which that only worked for a day. I have increased my pressure to 12ish psi, which didn't help at all.
I can still paint, but it gets annoying. That and I can't do candy coats because I can't get an even top coat wit the gun acting this way.
Any ideas?
While spraying, the powder comming through the gunn will slowly diminish. Then I('ll shake the gun (while still spraying) and then more will flow out, and then slowly diminish; the process repeats. Sometime without shaking it, the gun spits out a big cloud of powder. it seems the best wayt o keep a consistant stream is to continually shake the gun while spraying, but that gets tiring very quickly.
I only fill the cup up about 1/3 of the way, I have constant air at about 8 psi. I have 2 water seperators plus the water trap on the gun. I do live in a fairly humid climate. I shake the powder and check for clumps before attaching the cup to the gun. I have taken the gun apart to clean it to keep the trigger from sticking, which that only worked for a day. I have increased my pressure to 12ish psi, which didn't help at all.
I can still paint, but it gets annoying. That and I can't do candy coats because I can't get an even top coat wit the gun acting this way.
Any ideas?