    I have ben using flourescent orange for a while & really like the brightness without any base coat or polishing. Has anyone used Caswell's orange or Safety Orange? Are either close to the flourescent orange. I have some pics of the fl. orange in my photo album & the general Powder picture album. Check it out. Thanks for the input.


    nutty
    Last edited by ; 08-31-2005, 12:31 AM.
    SouthWest Powderworx
    Tyler Nutter
    5054803934
    www.swpowder.com
    myspace/swpowder
    [email protected]
    sigpic

  • #2
    Re: Anyone used Caswell's Safety Orange or Orange?

    Has anyone used Caswell's orange or Safety Orange?
    I've used Safety Orange:

    http://forum.caswellplating.com/phot...to=39&size=big

    Sean
    Seans Zinc Plating page

    Comment


    • #3
      Re: Anyone used Caswell's Safety Orange or Orange?

      not bad. was thast over a galvanized finish?


      nutty
      SouthWest Powderworx
      Tyler Nutter
      5054803934
      www.swpowder.com
      myspace/swpowder
      [email protected]
      sigpic

      Comment


      • #4
        Re: Anyone used Caswell's Safety Orange or Orange?

        Nutty:

        was that over a galvanized finish?
        Good question, I don't know right offhand. It was just one of many crufty old shackles I had around. I cleaned it and bead blasted it.

        I'll check the others later for galvanizing.

        Sean
        Seans Zinc Plating page

        Comment


        • #5
          Re: Anyone used Caswell's Safety Orange or Orange?

          I found a guy who gets powders made @ Prismatic & has a fl. orange done for him. I'm going to give it a try. Hey Caswell, get a bright fl. orange!!!