  • You know what would be helpfull.....

    Is if everyone who is powering an oven with a torpedo kerosene heater would post how many BTU's it is and what size oven it is heating up. This would show what the maximum space that a certain number of BTU's can handle and if someone already has a oven built this would show what size heater they are going to need. Or if somone knows off hand, what the biggest oven a 100k btu heater can get up to 400 degrees +, whats the biggest a 150k BTU can, 200k BTU, etc.....

  • #2
    Re: You know what would be helpfull.....

    I will keep searching my heater for the btu's, maybe i'll find it on the internet also? i'll get back to you guys.

    Comment


    • #3
      Re: You know what would be helpfull.....

      Any ideas? Man, this forum has been dead the last couple weeks.

      Comment


      • #4
        Re: You know what would be helpfull.....

        i cant find anywhere on the heater, there are specs stamped on to a thin plate on the side, but no-where does it say btu, only amperage, and all that jazz, if there is anything else i can look for i'll try.

        Comment


        • #5
          Re: You know what would be helpfull.....

          4'x6'x6' oven, 2" thick 6# density rockwool insulation, 150,000 btu propane torpedo heater. 520 degrees maximum temp.

          Leo
          www.tinmans.net
          "Life is not a journey to the grave with the intention of arriving safely in a pretty and well preserved body, but rather to skid in broadside, thoroughly used up, totally worn out, and loudly proclaiming -- WOW--What a Ride!!!" ----- Unknown

          Comment


          • #6
            Re: You know what would be helpfull.....

            Thanks a lot Leo, we need other people that have made ovens to give us there info. Cmon guys!

            Comment


            • #7
              Re: You know what would be helpfull.....

              4'x6'x4' 170,000 btu 3" thick walls with unfaced house insulation.