    Have a customer that is concerned with the high temp. He had a bad experience before with powdercoating on a automotive header catching fire.

    He was not sure if it was high temp.

    Is the high temp powder just for things that get warm? Or can you use it on something such as a snomobile, motorcycle, automotive exhaust manifold. I have only done mufflers with it so far.

    Thanks

  • #2
    Re: high temp- how high? - will it burn?

    my opinion is if doing exhaust, especially headers, you should be using techline coating. others may have had good luck with the high temp powder and will chime in i personally have not used high temp powder yet.
    when in doubt polish it out/ why replace it when you can refinish it
    G2 Polishing and Powdercoating

    Comment


    • #3
      Re: high temp- how high? - will it burn?

      The high temp has worked GREAT on the two mufflers I did. GREAT.

      But, I am not sure about the real high temps that an exhaust manifold will see.

      What is techline?

      Comment


      • #4
        Re: high temp- how high? - will it burn?

        http://www.caswellplating.com/aids/techline/index.html
        it is liquid coating that is good to 2000f. give the link a look see
        when in doubt polish it out/ why replace it when you can refinish it
        G2 Polishing and Powdercoating

        Comment


        • #5
          Re: high temp- how high? - will it burn?

          The techline is more a paint than a powder coating though, right?

          Comment


          • #6
            Re: high temp- how high? - will it burn?

            Originally posted by mtnbiker
            The techline is more a paint than a powder coating though, right?

            Yes, it is liquid.

            Comment


            • #7
              Re: high temp- how high? - will it burn?

              I've used the high temp on Car headers, bike headers etc with no problems..
              Even have it on my cars and Jeeps..