    Well I'm 99% sure I'm going to be purchasing PC equipment and I have one quick question. What is the heat durability of the non-high temp powders? I see the high-temp ones are good for 1000 F but havent found info on the other types of powder. Great site with tons of useful information. Keep up the good work.
    Thanks
    Adam
    Unorthodox Creations Powdercoating

  • #2
    Re: One quick question about PC heat durability

    I have tested generic powders to 300F plus with no issues. 400F in shorter intervals. 500F becomes kinda hit or miss. Depends on heat cycle.