  • Cleaning Oven

    Do any of you guys ever clean your ovens? I have been using mine for over 2 years and haven't cleaned it once. I recently noticed that there are specs of powder baked on the sides of the oven. I am fine with that, what bothers me is the powder that is baked on the glass. It is getting to the point where I am having a hard time seeing inside. Does anybody know of a cleaner that will get rid of the powder without scratching the glass?

  • #2
    Re: Cleaning Oven

    My suggestion would be to use some good soapy water (dish detergent will do fine) and a razor blade. Just don't get carried away with it and you shouldn't scratch the glass.

    David

    Comment


    • #3
      Re: Cleaning Oven

      The razor blade is what I used on glass doing paint & body.

      Comment


      • #4
        Re: Cleaning Oven

        on the big oven i got it has 2 glass doors and i have tried almost everything. razors with windex, mek, acetone, nothing seems to work so far. but best of luck with yours Captain i think mine has numerous layers of clear on it.i am about ready to try some aerosol stripper.
        when in doubt polish it out/ why replace it when you can refinish it
        G2 Polishing and Powdercoating

        Comment


        • #5
          Re: Cleaning Oven

          Captain, to eliminate dirt and specs I just blew out the oven before warming it up from time to time with an air hose. As for the old powder that is stuck in the oven, who cares, if it's stuck then it isn't airborn and thus not a problem.
          As for the window, buy a glass buffing kit and I think you'll be very pleased.

          Dale

          Comment