I powder coated my valve covers in reflective chrome and they came out great. I want to do anodized red over them..how much coverage should I put on? What temp should I bake them at? Also do I clear coat over that? What happens if I don't get good coverage on the anodized section first try can I go over it again? Any info is greatly appreciated...Thanks
Announcement
Collapse
No announcement yet.
Question about anodized red over reflective chrome??
Collapse
X
-
Re: Question about anodized red over reflective chrome??
I always do it in a 2 hand process and at 150 deg. of temp each coat
don't try to cover everything on first hand , if you see a powder less spot leave it or you will over build
second hand concentrate on those powder less spots and apply a general coat
my way to do it and has never failed me
you don't need clear