    Hello all. I am very interested in starting my own business. I am considering an Idea... How hard would it be to Create a "portable" station?

    Please tell me if you think this is possible...

    1.Small enclosed trailer (insulated) with strategic curing lamps.
    2.Air compressor
    3. Parts cleaner

    I know there are other things but I guess my Question is could a trailer double as a blast booth and a spray booth?

    Also My trailer would require adequate ventilation as well.


    CAN IT BE DONE

    if you have any Ideas email me At [email protected]

  • #2
    Re: Noob

    It can be done, I have seen it advertised before. You would need a blaster, generator, oven, powders, etc.... I dont think it is a good idea to have the blast booth double as a spray booth, too big of risk of contaminating parts.

    Comment


    • #3
      Re: Noob

      It seems like it would need a lot of electricity if you used curing lamps, unless they could run on gas.
      Steve Dold
      http://stevedold.com

      Comment


      • #4
        Re: Noob

        Any suggestions?

        Comment


        • #5
          Re: Noob

          If you are talking about Powder Coating I think your biggest problems would be powering your
          shop what is your idea for this .
          Then transport I would think possibly an old race car trailer so everything is inside what exactly
          are your thoughts . I believe anything can be done if you want it bad enough
          Jim Eaton

          Comment


          • #6
            Re: Noob

            This question crops up occasionally. Personally, I can never see the cash value or marketability of such a scheme. I doubt people are going to bring work to a mobile shop on a car show, and expect it to be done in a couple of hours.
            --
            Mike Caswell
            Caswell Inc
            http://www.caswellplating.com
            Need Support? Visit our online support section at http://support.caswellplating.com