Re: Caswell's Professional Powder Coating System
"Choosing the right application package will depend on the nature of
the task. The corona gun, tribo gun, the bell, and the disc are all tools
that can meet certain requirements. No single tool is perfect for every
powder application.
A corona-charging gun offers more methods of adjustment for differences
in part size and geometry. Air flow patterns, powder volume,
velocity, and voltage level can be adjusted to accommodate different parts and powders.
This gives the operator a lot of flexibility in controlling
film thickness, dealing with Faraday cage and other process
variables that are common in production facilities. The use of discharge
voltage creates field lines and a highly ionized electrical field
that can cause a variety of application challenges.
Generally, a tribo system will work best in situations where there is
not a lot of variety of parts and powders. With a tribo gun, the powder
volume can be adjusted and the gun to target distance can be adjusted.
The best application for tribo guns is one where there is little
or no need for adjustment. One powder and a fairly consistent mix of
parts can be run very effectively with a tribo gun. Used with the correct
powder material, the tribo gun can be very effective. Testing should
be conducted to be sure that the powder material is compatible with
this positive charging device.
Most powder operations in North America use the corona-charging
gun to take advantage of the flexibility of voltage control and ability to
spray any thermoset powder effectively. In Europe more tribo spray
guns are used to take advantage of the penetration characteristics."