    Folks think your going to like this one. Here is a sample showing a Reflection of my cig pack.. No this is not cleared yet withthe super clear, will do this later today.. But this is getting real close to chrome...

    Jim S...
    Attached Files
    Jim Shuster
    www.backyardpowdercoating.com Sold.....
    www.chrissys68mustang.com Hobbie
    www.photogserver.net Web Hosting.

  • #2
    Re: Xtreme Chrome...

    That looks really good! It will be interesting to see how the clear works.

    Comment


    • #3
      Re: Xtreme Chrome...

      well, that stuff is on my next order, it looks great, alot better than the otherones even without the clear, hopefully it holds it's look with the clear.

      Comment


      • #4
        Re: Xtreme Chrome...

        I also want to see what it ends up like after the clear coat.

        I also want to try the one step chrome that is out there now.

        Comment


        • #5
          Re: Xtreme Chrome...

          All chrome powders are one step chrome...if, and only if the part is not exposed to the elements.

          There is not a chrome powder in existance that doesn't need a clearcoat if it's for outdoor use.
          --
          Mike Caswell
          Caswell Inc
          http://www.caswellplating.com
          Need Support? Visit our online support section at http://support.caswellplating.com

          Comment


          • #6
            Re: Xtreme Chrome...

            I have to trust you on that. But, I thought I remember reading it somewhere.

            Comment


            • #7
              Re: Xtreme Chrome...

              There are companys that now sell a single stage chrome that is very impressive.

              Comment


              • #8
                Re: Xtreme Chrome...

                Originally posted by tavo1765
                There are companys that now sell a single stage chrome that is very impressive.
                Our Tiger Drylac rep, who has 20+ years in the PC industry, and I talked at length about this, because I wanted to start stocking this "magic" chrome powder, and I was assured that single stage chrome is not 100% truthful because if the parts are exposed to the elements, they will oxidize and fade over time. Clearcoats are absolutely necessary to prevent oxidization.

                I guess we could call our chrome powders single stage chrome, then put in the tiny, tiny small print indoor use only, but I prefer to be honest with people about what they're getting.

                If anyone has any real experience with one of the chrome powders marketed as single stage, and can show that after 6+ months of outdoor use it still looks shiny, I'd be more than happy to look at the product again.
                --
                Mike Caswell
                Caswell Inc
                http://www.caswellplating.com
                Need Support? Visit our online support section at http://support.caswellplating.com

                Comment


                • #9
                  Re: Xtreme Chrome...

                  The single stage chrome powder I buy is holding up pretty damn good since last year which the coated items are exposed to the bay arear of Brooklyn NY. I coated titanuim railings about 40ft long with this stuff and no clear coat, buyer did not want it because of the additional price. But all metallics require a top coat, your correct in saying that to your customers. But I can stand behind this so called single stage powder since I use it all the time now, also I have been running a powder coating business for a few years now, this may have something to do with why its lasting since it was chemically pretreated.