Would it work to powdercoats cylinders for a snowmobile? Some here in north of Sweden race a lot and its not that hard for them to get over 250 hp out of then, so the question is, would powder work for it? I would normally ceramic coat them, but in this case the owner wants more for the eye than black coating.
Announcement
Collapse
No announcement yet.
Snowmobile cylinders?
Collapse
X
-
Tags: None
-
Re: Snowmobile cylinders?
I do jugs all the time, no problems.. Just do not get it inside...
Jim S...Jim Shuster
www.backyardpowdercoating.com Sold.....
www.chrissys68mustang.com Hobbie
www.photogserver.net Web Hosting.
-
Re: Snowmobile cylinders?
no prob on the jugs for sure...but if you want to do the insides or pistons theres some stuff called Thermo Dyne....just to keep good ol Caswell Happy if you e-mail me I'll tell you were you can get it ...