Re: Wrinkle Red help
Once you know the part is actually to temp..."for sure". That's one of the problems with the smaller ovens, they heat up to quick and the part never see's the temp it needs.
I'd do 400 for 25 mins.
You can see the thicker areas of the part is kind of shinny.
IMHO
Announcement
Collapse
No announcement yet.
Wrinkle Red help
Collapse
X
-
Re: Wrinkle Red help
so I should cure for more then 20 min's? what temp and time would you suggest?
Leave a comment:
-
Re: Wrinkle Red help
Check this out. It also has an URL in the last post that might help.
http://forum.caswellplating.com/showthread.php?t=3380
Leave a comment:
-
Wrinkle Red help
I bought some wrinkle red powder and cannot seem to really get the wrinkle I should be out of it. I have tried it 2 times. first time at 400 for 10 min's second time I tried it at 350 for 20 min's both times it came out looking like this. Anyone have any idea's of what I would be doing wrong?
Tags: None
Leave a comment: