    Re: Screen your powder

    We haven't ever screened any powder, a couple minutes in the fluidizing hopper and it about doubles in volume.

    Leave a comment:


  • callmej75
    replied
    Re: Screen your powder

    What I do, if I purchase some powder thats in a box, I just roll the box around til the powder is "loose" rather than breaking it out and using it. We use to screen it til the powder supplier told us to roll the boxes til the powder was fine.

    Leave a comment:


  • kchotboat
    replied
    Re: Screen your powder

    I use a flour sifter.

    Leave a comment:


  • BigDog
    replied
    Re: Screen your powder

    Originally posted by myillwillinc
    where do i get a good supply of mesh screen? everywhere i go they look at me funny. i can't get them to understand down here what i'm lookinh for.
    Try this link: http://www.bigceramicstore.com/supplies/Sieves.htm

    Leave a comment:


  • myillwillinc
    replied
    Re: Screen your powder

    where do i get a good supply of mesh screen? everywhere i go they look at me funny. i can't get them to understand down here what i'm lookinh for.

    Leave a comment:


  • BigDog
    started a topic Screen your powder

    Screen your powder

    Does anyone do this?

    The most common reason that powders puff and surge during application is due to the lack of screening. Powders may become compressed in transportation or in storage and will form large compacted groups of particles that will clog up feed hoses.
    Screening of powders, new and reclaimed, will insure uniform particle size distribution, separate out contaminants, and allow the system operator to fine tune the application equipment without puffing or surging for maximum transfer efficiency and finish quality. Actual on-line test results have shown that screened powder will cover much more area than the same material unscreened. Powder should be screened into a clean dry hopper. Powders are manufactured by the manufacturer through an 80 mesh screen. The powder is light and fluffy when they make it. It may not be light and fluffy when you get it at your facility. If the powder manufacturer is screening though an 80 mesh screen, and you screen through a standard stainless steel window screen, the powder should fall through just as fast as you pour it in. That's going to prevent you from introducing into your system, balls of coagulated powder that are going to clog your feed lines. What happens when you clog your feed lines? You get puffing and surging.

    When jobs require a Class A surface, that is a blemish free or near blemish free surface, depending on what Class A means to the customer who's defining Class A, it is wise to pour the powder through a 100 mesh screen. A 100 mesh screen is tighter than the 80 mesh screen the powder manufacturers use to make their powder. But what you are doing is taking out all the heavy particles. And when you spray that powder, you can get a near blemish-free surface.
    Last edited by BigDog; 02-25-2006, 12:39 AM.