    a cheap but very effective way to degrease clean and strip I found was to use a old metal garbage can and fill it with enough water to do your parts in...just add a can or two of good old crystal drano and mix it well...make sure you use the crystal stuff and not the liquid stuff...I added a old drill with one of those long paint mixer attachements to agitate the stuff...

    BTW sorry havent been around been busy and playing for a change....
    Pro-Tech Powder Coating
    93976 Ocean Way
    541-247-8168
    [email protected]
    Gold Beach,Oregon

  • #2
    Re: Down and dirty

    Yea, that's basically sodium hydroxide (lye). Be careful using that on aluminum or zinc die cast, it will attack the metal.