I have three water separator on my set up. One in the basement right off the compessor, the next one right when the airline gets in the garage and then one at my booth. two of the three have regulators and a small one at the gun.
Announcement
Collapse
No announcement yet.
Running 2 regulators?
Collapse
X
-
Re: Running 2 regulators?
It will not hurt to run a second regulator inline.
Leave a comment:
-
Running 2 regulators?
Is it ok to run 2 regulators on a compressor? I have the regular regulator on the compressor but I also have an oil/water separator that also has a regulator on it too. Not sure if I should hook up both or what. I believe the regulator on the air compressor goes beyond 70psi but the other regulator with the separator only goes up to 70psi max. I am getting some really small fisheyes on my test panels and was hoping this would be the fix.Tags: None