Is it ok to run 2 regulators on a compressor? I have the regular regulator on the compressor but I also have an oil/water separator that also has a regulator on it too. Not sure if I should hook up both or what. I believe the regulator on the air compressor goes beyond 70psi but the other regulator with the separator only goes up to 70psi max. I am getting some really small fisheyes on my test panels and was hoping this would be the fix.