I have been having problems with getting the Silver Vein Look to come out even. I have tried to make sure the coating is applied evenly, but still can't get a consistant pattern to the final product. Any suggestions? I have cleaned prepped as best I can but still get the same results! Anyone else experience these problems?
Announcement
Collapse
No announcement yet.
Silver Vein Issues
Collapse
X
-
Re: Silver Vein Issues
Try heating it at a lower temp. I have used this powder befor and never had a problem with it, but I did have a problem with the Black Wrinkle for a lone time till I cured it at a lower temp. Try 8-10deg lower then what your doing it at but then you mite want to leave it it a lttle longer too like 8min I would think.WARCHILD