    Re: satin black

    Yup, what sswee said, I use it alot, looks great.
    mach

    Leave a comment:


  • baz
    replied
    Re: satin black

    thanks sswee just checked your gallery , exactly what i want . you saved my day ,now i hope caswell has in stock in their canadian warehouse

    Leave a comment:


  • sswee
    replied
    Re: satin black

    baz,
    You might want to check out the Black Cat Urethane. It has the look your describing. I use it on many parts doing restorations. There are quite a few pics in my album with it.
    SS

    Leave a comment:


  • baz
    replied
    Re: satin black

    not really what i want , this link is for high temp paint , i just need regular power
    to coat some vave covers , but with a satin look , not a gloss black and not a flat black ,

    Leave a comment:


  • lcaswell
    replied
    Re: satin black

    Black Satin Header Coating
    http://www.caswellplating.com/aids/techline/index.html

    Leave a comment:


  • baz
    started a topic satin black

    satin black

    do caswell carry a satin black powder, if so i can not find it on the site or in catalog , under what name would it be.and if anyone has tried it ,what kind of results did you get.
    thanks
Working...
X