  • New Hobby System- Motorcycle frame??

    Will it handle something as big as a motorcycle frame?

  • #2
    Re: New Hobby System- Motorcycle frame??

    Yes, I've done 2 motorcycle frames and a quad frame. 2 in chassis black and one safety red. They came out great.

    Comment


    • #3
      Re: New Hobby System- Motorcycle frame??

      Ya, it's not really the gun that dictated what you can do, it's your oven. Doesn't really matter if you can spray it, unless you can bake it
      Dan Pesonen
      Bandit Powder Coat <<From Powder to Perfection>>
      Forest Grove, BC Canada

      Personal motto:
      "If it ain't broke, modify somethin till it is"

      Comment


      • #4
        Re: New Hobby System- Motorcycle frame??

        Originally posted by Millermatic
        Yes, I've done 2 motorcycle frames and a quad frame. 2 in chassis black and one safety red. They came out great.
        Thanks.

        Comment