    which of the 3 chrome powders look the best when clearcoated?
    Xtreme, Near or Super?

  • #2
    Re: Chrome Powders?

    Personally, I have only used Extreme, and I find it goes more of a satin, or brushed aluminum after a month with clerarcoat. I have tried all ways to spray, clearcoat hot, half baked, full bake, cold, etc.
    Dan Pesonen
    Bandit Powder Coat <<From Powder to Perfection>>
    Forest Grove, BC Canada

    Personal motto:
    "If it ain't broke, modify somethin till it is"

    Comment


    • #3
      Re: Chrome Powders?

      i've only used the extreme, too (based on information on this forum that said it's the best of the three). as initially shot, it's almost ok. once clear coated it's a glossy grey. expect to be disappointed.
      Len
      Figure Finishing
      www.FigureEngineering.com
      866-900-4949

      Comment


      • #4
        Re: Chrome Powders?

        i have used the 3
        not that they look like chrome but
        best one with clear is xtreme chrome
        super chrome end up like a reflective light silver
        near chrome ends up like a solid silver

        but for candys I love super chorme
        Last edited by jtagger19; 08-05-2007, 08:57 AM.

        Comment


        • #5
          Re: Chrome Powders?

          Originally posted by jtagger19
          but for candys I love super chorme
          yes, i sounded too down on the chromes. it is great for candies. have you found super chrome to be better for candies than xretme chrome?