    Originally posted by Harleydad View Post
    After the sanding I'd blow it off with clean,dry air.

    i'm assuming we're all not completely inept @ this whole thing.

    Leave a comment:


  • Spitfire13
    replied
    Re: 2nd Coat Question

    It sounds like you could be having a transfer efficiency problem. The 2nd coat might be a little thin. A thin coat will give you a rougher, tight orange peel effect. Do you have a gage to check your cured powder thickness?

    Leave a comment:


  • Harleydad
    replied
    Re: 2nd Coat Question

    Originally posted by bradnailer View Post
    sand with what grit?
    220 should work for ya.

    Leave a comment:


  • bradnailer
    replied
    Re: 2nd Coat Question

    sand with what grit?

    Leave a comment:


  • Harleydad
    replied
    Re: 2nd Coat Question

    Originally posted by nuttyman View Post
    that happens with glossy powders. 2nd coat glossy's can be tough. if a 2nd is needed w/ a glossy powder let it cool, sand & apply over the whole thing.
    After the sanding I'd blow it off with clean,dry air.

    Leave a comment:


  • nuttyman
    replied
    Re: 2nd Coat Question

    that happens with glossy powders. 2nd coat glossy's can be tough. if a 2nd is needed w/ a glossy powder let it cool, sand & apply over the whole thing.

    Leave a comment:


  • donafams
    replied
    Re: 2nd Coat Question

    50kv gun, respraying the whole piece, warm, like about 160deg, not sanding between spraying

    Leave a comment:


  • Harleydad
    replied
    Re: 2nd Coat Question

    Are you trying to just touch up the light spot or do you cover the whole part? Are you sanding between coats and are you spraying them hot (hot flock) or cold?
    Do you have an adjustable kv gun?

    Leave a comment:


  • donafams
    started a topic 2nd Coat Question

    2nd Coat Question

    ive noticed that first coats go on very smooth, but if i missed a small spot, and decide to spray a 2nd coat its not as smooth as the first. first is almost like glass and the 2nd is a little rougher. is this normall with powder on top of powder or is there a trickto nicer 2nd coats?