i was was just wondering how much powder does it usally take to coat 4 wheels.i've never done any wheels yet,and a customer wants some done.
Announcement
Collapse
No announcement yet.
Wheels
Collapse
X
-
Re: Wheels
i saw someone post 2lb for 4 17in car rims.
Comment
-
Re: Wheels
2 lbs is plenty for 4 17" wheels.SouthWest Powderworx