  • Will clear PC prevent rusting on steel?

    I have an axle, a-arms and ti-rods off of my ATV that are chromed steel. What I would like to know is, if I was to clear PC them will that prevent rust because they have some rust spots here and there. Let me know what you think.
    Thanks

  • #2
    Re: Will clear PC prevent rusting on steel?

    if you remove the rust first then yes. must be a lousy chrome job or very old.
    SouthWest Powderworx
    Tyler Nutter
    5054803934
    www.swpowder.com
    myspace/swpowder
    [email protected]
    sigpic

    Comment


    • #3
      Re: Will clear PC prevent rusting on steel?

      Yeah it's pretty old. If I was to polish it up real nice before PC and then clear coat it, would it dull the chrome and polish?
      Thanks

      Comment


      • #4
        Re: Will clear PC prevent rusting on steel?

        dulling will be minimal. test on a piece that's inconspicuous to see if it's acceptable to you.