I am very happy with the way it came out! Columbia SS Chrome. Outgassed for 1 hr, PC'ed at 140 degrees and cured at 375 for 20 min. The intake had a pretty rough blast finish when it was delivered.
Announcement
Collapse
No announcement yet.
1st Intake Manifold!!!
Collapse
X
-
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
[email protected]
sigpic
Comment
-
Re: 1st Intake Manifold!!!
Just got the gloss clear today...DO I need to reheat the SS chrome PCed manifold before I shoot the clear coat? Any tips would be appreciated. Don't want to F it up.GatorHyde of Denver
10650 Irma Dr. #24
Northglenn, CO 80233
303 280-3056
Comment
-
Re: 1st Intake Manifold!!!
You know customers...they always want everything to look "perfect". He says the SS chrome is not glossy enough and wants a gloss clear shot on it. I just don't want to F it up and have some cloudy effect happen. I know not to put the clear on too thick...I did it yesterday over Black Chrome on a test panel and had disaster throw away junk results. Just wondering if I should reheat the mainfold to say maybe 140 and pull it out to shoot the clearGatorHyde of Denver
10650 Irma Dr. #24
Northglenn, CO 80233
303 280-3056
Comment
-
Re: 1st Intake Manifold!!!
For what it's worth GatorHyde, I think it looks pretty sharp! After some looking around, I don't think that the chrome colors really get much more reflective than that, do they? Keep us posted about the clear! I'd give you my two cents, but I don't have that much in my pocket yet, just started up my powder coating.
Best of luck!
~Josh
Comment
-
Re: 1st Intake Manifold!!!
Originally posted by GatorHyde View PostYou know customers...they always want everything to look "perfect". He says the SS chrome is not glossy enough and wants a gloss clear shot on it. I just don't want to F it up and have some cloudy effect happen. I know not to put the clear on too thick...I did it yesterday over Black Chrome on a test panel and had disaster throw away junk results. Just wondering if I should reheat the mainfold to say maybe 140 and pull it out to shoot the clear
Comment
-
Re: 1st Intake Manifold!!!
Originally posted by JTW37 View PostIsn't that a Single Stage Chrome? If it is, why would he want to clear it also?
http://forum.eastwoodco.com/showthre...me+powder+coat
Comment