  • spray booth

    how come i dont see any powder coating spray booths that are enclosed?

  • #2
    What do you mean enclosed ? Like no place to let air out ? If you think of all the air you actual forces into a cabinett, you would have a lot of dust just storming around in the air, if you didn`t have a place du evacuate all the air you push inn...

    Maybe I didn`t understand your question.
    Did you know that it is possible to use every gram of powder if you recycle when coating, and vapors are almost none !
    In a wet paint approx. 80-90 % evaporates into the air. Causing stress on the enviroment !
    1 kg. of powder can cover approx. 10-12 m3
    1 litre. of wet paint covers approx. 2-3 m3