    started a topic air tight oven vs vented oven

    air tight oven vs vented oven

    another thing i am confused about. I read about how you want a nice air tight oven with a door seal...... but then i read you should vent your oven... how does this work.

    What is the purpose of venting besides letting fumes out? does the air expand that much during heat up? How does one vent an oven without loosing all the heat like a chimney?

  • JTW37
    replied
    Re: air tight oven vs vented oven

    Make sure you only use around a 1/2 dia. pipe, 1 or 2 inches.

    Leave a comment:


  • bikerdad46
    replied
    Re: air tight oven vs vented oven

    Originally posted by purpony View Post
    another thing i am confused about. I read about how you want a nice air tight oven with a door seal...... but then i read you should vent your oven... how does this work.

    What is the purpose of venting besides letting fumes out? does the air expand that much during heat up? How does one vent an oven without loosing all the heat like a chimney?
    Hello purpony
    Yes you need the oven vented. Just install a 1 to 2 inch pipe through the top with a couple of 90*s to form a upside down U. That lets the expanding air out.
    bikerdad46