  • edwardpic
    replied
    Re: Where to get insulation?

    you can get mineral wool which is used in furnaces from McMaster-Carr. We just built a 4X4X6 oven using 2" of 1800 degree insulation---cool to the touch on the outside when running at 400 degress

    Ed
    Have pics of ove email me and i will send, can also provide part numbers of all the items used in our oven!!

    Leave a comment:


  • DJuanHouston
    replied
    Re: Where to get insulation?

    Originally posted by sab0276
    Are you talking about the Dow Tuff-R R13 Insulation at Home Depot.

    Any problems? Melting/burning/smoking?

    -Scott

    I wondered the same thing cause the msds says 190F but i bet thats just because of the coating they pealed off

    Leave a comment:


  • Heavykote
    replied
    Re: Where to get insulation?

    I hit a Home Depot today and picked up water heater insulation. I am gonna take some plywood and wrap the insulation which is double foil backed and use some kind of adhesive to apply. Then, I can connect the pieces for my oven extension. It should work, right?

    Leave a comment:


  • sab0276
    replied
    Re: Where to get insulation?

    Originally posted by kd5sfq
    Call me cheap but mine came from Home Depot. I used R-13 wall insulation and removed the plastic wrap. The fiberglass has a melting point of 1,000 degrees F. So it's okay to use. Domestic ovens use the same type of insulation.
    Are you talking about the Dow Tuff-R R13 Insulation at Home Depot.

    Any problems? Melting/burning/smoking?

    -Scott
    Last edited by sab0276; 01-06-2006, 02:27 PM.

    Leave a comment:


  • KZjim
    replied
    Re: Where to get insulation?

    try McMaster/Carr they have 1000deg blankets that are 3/4" thick

    Leave a comment:


  • sdold
    replied
    Re: Where to get insulation?

    Same here, I bought the stuff with kraft paper, and just peeled the paper off. It seems to work well in initial tests.

    Leave a comment:


  • kd5sfq
    replied
    Re: Where to get insulation?

    Call me cheap but mine came from Home Depot. I used R-13 wall insulation and removed the plastic wrap. The fiberglass has a melting point of 1,000 degrees F. So it's okay to use. Domestic ovens use the same type of insulation.

    Leave a comment:


  • gourdhedd
    replied
    Re: Where to get insulation?

    I used a 2" thick, 3 PCF unfaced fiberglass board for my oven. The same product is manufactured by Owens-Corning, Knauf, Johns-Manville, and Certainteed. Do a google search to find their websites and then look for a "Where to buy" page. This should lead you to a local distributor. You can also do a google search for "General Insulation" to find out if they have a warehouse close to you.

    I paid about $66 for an 80SF bundle.

    Gary

    Leave a comment:


  • cdaeme
    replied
    Re: Where to get insulation?

    If you live in or arround a moderate size city check the Yellow pages for insulation suppliers. I called around yesterday found a local supply house that carries Mineral Wool (aka Rock Wool) for $2.49 for a 2'X4'X1 1/2" sheet.

    While talking to the salesman on the phone he asked what I was using it for the discussion then changed to powder coating. He wants me to look at coating some Jr. Dragster parts while he is doing his winter rebuild.

    Jason Williams
    Auto-Cycle PC
    Chattanooga, TN

    Leave a comment:


  • remotestartdepot
    started a topic Where to get insulation?

    Where to get insulation?

    I know a lot of you are using that foil backed foam board, but the local Home Depot don't seem to carry that stuff. Where is the best place to find that stuff and what should I expect to pay? Also, is there anything else that I can use for insulation? Will good ole Pink Panther fiberglass insulation work, or will it burst into flames.