Re: Element placement for a vertical oven?
I'm planning something very similar. I will use 4 elements, 2 upper & 2 lower. I will put a divider in between so I can use only 1 oven if needed for smaller parts / batches. I'm going to put 1 element on each side of the bix & the temp probe centered on the back panel if at all possible.
Announcement
Collapse
No announcement yet.
Element placement for a vertical oven?
Collapse
X
-
Element placement for a vertical oven?
Ok im looking to build my own oven, I need an upright oven due to space issues The horizontal oven would take up more space then I can spare. So my question is where to place the elements? Im looking to have a 60x36x36 oven and i want it to be an upright. Thanks for the help in advance.
JHFTags: None
Leave a comment: