Announcement

Collapse
No announcement yet.

My oven

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • My oven

    I got the Idea from this dude. But I'm a fat dude so I wanted to make it upright. I used a old cabinet like you would see in a old school and the barn door track things real cool. That was my idea. I'm new to this site I hope you can see the pics.
    http://www.powdercoatoven.4t.com/Index.html
    Attached Files

  • #2
    Re: My oven

    If you have any questions e-mail me at [email protected]
    Attached Files

    Comment


    • #3
      Re: My oven

      good job man. I was just thinking about that today. I actually thought about putting two of those together to make it a twice as deep. What did you use to insulate it?

      Comment


      • #4
        Re: My oven

        That looks real good Mike...

        Looks like fiberglass duct board for insulation

        Comment


        • #5
          Re: My oven

          The insulation is Owens Corning 2" 703 from there 700 series. It comes in 2x4 sheets 96sf in a box. I'm still waiting for the contactor to come in from Famous parts .com. I have the thermostat controlling a light bulb so I now when shut off the breaker until the contactor comes in. I got the basic idea from that web site he gives a lot of info on materials and stuff. I could'nt get the contactor cheaper local. All you need is two old ovens and your in. I used metal studs to build two boxes to mount the elements in the bottom. The only thing I can't seem to come up with is a circulation fan I keep drawing a blank on that one. But it works good heats up in 10 min. and runs one more time for a few min. Thanks guys.
          Attached Files
          Last edited by mikekozura; 02-11-2006, 10:06 AM.

          Comment


          • #6
            Re: My oven

            Mike,
            Don't know where you're out of but you should have an electric motor shop somewhere close by. The usually carry some small motors and small fan blades. We used a cheap air over 1/16 hp motor a 5 or 6" fan blade inside the cabinet. Shaft goes through the side wall and mounted the motor outside the cabinet. We got one with the shaft plenty long and mounted a 4" fan blade and 2" (cut down a 4") fan on the shaft between the cabinet and the motor. The inside one circulates the air and the 4" blows air over the motor and the 2" acts like a heat sling.
            Motor has been chugging away for 2 years, the works cost about $50..
            The motor shop can help you pick the motor and blade so you get the rotation and correct blades..

            Hope that helps

            Comment


            • #7
              Re: My oven

              I'm live 20 miles south of Pittsburgh, PA. baby home of the World Champs. HERE WE GO STEELERS HERE WE GO. Thanks for the info I got some things brewing in my head now and that was a big help. Don't know where your from but I hope your a STEELER fan. LOL

              This site has been a lot of help at least people will talk to you. I bought some powder from Pendry and was on there site and no one would talk to me.

              This powder coating and polishing is just like anything else common sense, practice, and what works for you. But its nice to have somewhere to turn for a opinion from someone that knows what the [email protected] there doing. Thanks again.

              Comment


              • #8
                Re: My oven

                I've got to agree with you, pretty sociable bunch here and some very knowledgeable members too.
                We're situated about 50 miles due South of Cleveland. Not much of a football fan anymore but I can tell you when the Browns and Steelers play I know who will win

                Comment


                • #9
                  Re: My oven

                  Originally posted by Popeye
                  We're situated about 50 miles due South of Cleveland.
                  Being from the Pittsburgh area sorry to here about you being from Cleveland. Just kidding LOL LOL You sound like a [email protected] of a nice person. Thanks again

                  Hey, I got a good idea who would win too. HERE WE GO STEELERS HERE WE GO

                  Well I have to go and put some powder on some quad parts. Talk to you later.
                  Last edited by mikekozura; 02-11-2006, 01:19 PM.

                  Comment


                  • #10
                    Re: My oven

                    I'm just playing now. I'm going to try posting a pic from my kids web page.