    the mineral wool panels are 2" thick and 24" X 48" part number from McMaster-Carr is: 9328k43 and run about $7 per panel, cheaper when you buy a case which is 5

    Ed

    Leave a comment:


  • edwardpic
    replied
    Re: Just Finished

    we used mineral wool insulation from McMaster-Carr. with the digital controls our oven ran around $1300....i have part numbers and prices if you email me i can send pictures, tried to post them here but the files were too large

    Ed

    Leave a comment:


  • DJuanHouston
    replied
    Re: Just Finished

    yeah my next buy wil be the insul, but Im not sure about the R13 on the other post, what did you use and cost wise?

    Leave a comment:


  • edwardpic
    started a topic Just Finished

    Just Finished

    We just finished our oven. 4X4X6, running 3 phase-6 1500W elements wired in Delta. Digital Controller-Draft inducing fan-reaches 475 no problem.
    Will take pictures and post soon, or you can email me at: [email protected] and i can send you some. I can also help with: insulation-part numbers-items used.