    Can i use a toaster oven to start powder caoting(smal items\wrenches)..i am totaly new and want to start small as not to get discouraged.

  • #2
    Re: a little help please

    by all means. i have 3 ovens, a big 3x5x6, a house oven and a small toaster size convection oven. the toaster is great for small parts and will be a great way to start out. welcome and best of luck bro.
    when in doubt polish it out/ why replace it when you can refinish it
    G2 Polishing and Powdercoating

    Comment


    • #3
      Re: a little help please

      thank you and hopefully they turn out..

      Comment


      • #4
        Re: a little help please

        hi im brand new to coating , if u use household oven how do u circulate the air thanks great learning tool

        Comment


        • #5
          Re: a little help please

          A regular oven is approx. 17" x22". and also it is vented at the top, so I dont think you need to circulate the air. I think I circulate to much air by opening and closing. Im always looking.

          Comment


          • #6
            Re: a little help please

            pootsman55 is correct. Smaller home style ovens really do not need air circulation simply due to size. Bigger ovens need fans to prevent cold spots inside the box (which is only bad if the part is residing in that area).