  • pokchop
    replied
    Re: How to get the best look

    Thanks guys. I have a silver hybrid metallic with a [email protected] load of flakes.

    Leave a comment:


  • mikekozura
    replied
    Re: How to get the best look

    Originally posted by pokchop
    Hey guys can anybody tell me how i can get the best look from the candy red translucent.Wich base color should i use..
    I've only used silver metallic, on Kyle's frame man you should see it out in the sun I was washing it today for the first time man with the water and the sun...sweet. If thats the look your looking for that silver has a [email protected] load on metallic in it. You can't see from the pics but belive me it's sweet.
    Attached Files

    Leave a comment:


  • pickleboy
    replied
    Re: How to get the best look

    i get a real good look from a chrome base. you can also use gloss white.

    Leave a comment:


  • pokchop
    started a topic How to get the best look

    How to get the best look

    Hey guys can anybody tell me how i can get the best look from the candy red translucent.Wich base color should i use..
Working...
X