Re: Insulation Thickness
I have installed the insulation.. wow the garage is nice and cool now...LOL anyway..
here is the info from the bundle just incase anyone needs it...
Rock Wool Manufacturing Co.
PO Box 506
Leeds, AL 35094-0506
Tel; 205.699.6121
and a link to the standard
Announcement
Collapse
No announcement yet.
Insulation Thickness
Collapse
X
-
Re: Insulation Thickness
More is better in this case- Most commercial ovens use at least 4" so you could go either way but if the cost difference is not an issue (depending on the oven size) then I would go with the 6" - keeping in mind that you want the insulation to have some room to breathe- Dont pack it like 10#'s of doo in a 5# bag.....
Leave a comment:
-
Insulation Thickness
I'm ordering 3" rock wool insulation today.. should i double it? make it 6" instead? any opinions?Tags: None