Does anyone have any experience with PID Temp controllers like those from
www.auberins.com?
They look like a lot of capability for the cost! The 30 step one can be programed to not only maintain temp. but to ramp up , soak, and shut down on a schedule. They also said more than one program can be saved and recalled.