Re: insulation help
We got ours at a local drywall supply house, along with the steel studs, very good prices!
Mike
Sho Me Coatings
Announcement
Collapse
No announcement yet.
insulation help
Collapse
X
-
Re: insulation help
FSTFBDY, did you get yours at a lumber yard too? How thick is yours?
Leave a comment:
-
Re: insulation help
Originally posted by edwardpicif all else fails, McMaster-Carr has mineral wool, thats where we got ours for our 4x4x6 oven
Leave a comment:
-
Re: insulation help
if all else fails, McMaster-Carr has mineral wool, thats where we got ours for our 4x4x6 oven
Leave a comment:
-
Re: insulation help
Rock Wool Manufacturing Co.
PO Box 506
Leeds, AL 35094-0506
Tel; 205.699.6121
Leave a comment:
-
Re: insulation help
Larger lumber yards or contracting supply houses. Usually comerial drywall contractors know where to get it.
Leave a comment:
-
Re: insulation help
mineral wool here for my new oven also.
its 29bucks a bundle. (9) 2x4 sheets
Leave a comment:
-
Re: insulation help
I recently built an oven based on the designs of a few large manufaturers and I used mineral wool insulation. It has a temp rating of 2900 deg. I got it at a drywall supply house and it was relatively inexpensive. It is also known as rotten cotton in the construction trade. It was 3" thick and 2'x4'. hope this helps out.
Leave a comment:
-
insulation help
my preg.oven has 22 gauge metal and i wraped it with a/c foil backed isulation. my problem is the isulation is getting very,very hot.should i get some other type insulation for inside the oven?it is bare metal inside my oven.with the isulation wraped around the new addition. what do i need to do?Tags: None