  • edwardpic
    replied
    Re: oven pics

    Thanks, we are building a bigger one and will be seilling that one. Yes the controller is PID and can be programmed to do many things, although basic target temperature and current temp is all thats really needed least in our case. Below is a list of parts-prices etc for most of the parts used except for the steel and wire.

    McMaster-Carr parts below

    Enclosure 18x18x8
    75065k43
    60.82

    Contactor 240V 3-pole
    6564k83
    55.26

    Main disconnect Panel Mount
    6759k233
    53.48

    Power Distribution Block
    7626k33
    37.02

    Thermostat
    Digital
    38615k11
    188.42

    Dial-IF DIDGITAL IS NOT WANTED
    33215k22
    92.12 connector # 7122k19 4.20 needed for operation

    Thermo coupler
    Type J
    3871k91
    37.22

    Mineral wool
    #9328K43

    Gasket
    #8815K42

    Fan from Grainer
    4MH08
    __________________________________________________ ________
    Cheaper PID controller can be bought here
    http://auberins.com/


    Hope that info helps-took me awhile tp make the pics smaller to post here!!!

    Leave a comment:


  • planebuilder
    replied
    Re: oven pics

    Excellent work!!! I noticed the controller, I assume it's a PID. Can you program ramp, soak , shutdown etc.
    Could you list details/sources for the controller, SSR, switch.
    Thanks

    Leave a comment:


  • edwardpic
    replied
    Re: oven pics

    controller and the fan system---it draws from the top ducted down the back of the oven and then enters at the bottom for a pretty even air flow...fan is 315 CFM and im thinking of adding another
    Attached Files

    Leave a comment:


  • edwardpic
    replied
    Re: oven pics

    more ok this should do for now...till i can get more
    Attached Files

    Leave a comment:


  • edwardpic
    replied
    Re: oven pics

    ok maybe a little larger photo's...bear with me guys
    Attached Files

    Leave a comment:


  • edwardpic
    replied
    Re: oven pics

    hope these work too
    Attached Files

    Leave a comment:


  • edwardpic
    started a topic oven pics

    oven pics

    sorry took so long, have been swamped here at the shop, and have been filming a TV show that will air on speed channel. hope these work had to resize them to post here
    Attached Files
Working...
X