    I was woundering if a dryer heating element will work in my oven?

  • #2
    Re: dryer element

    doubtful-I don't think it would reach the necessary temps.
    SouthWest Powderworx
    Tyler Nutter
    5054803934
    www.swpowder.com
    myspace/swpowder
    [email protected]
    sigpic

    Comment


    • #3
      Re: dryer element

      Can you post a picture of this element? Does it have the wattage embossed on the element somewhere?

      If you know the wattage, I can help you decide what size of an oven it would be able to heat up....

      Comment


      • #4
        Re: dryer element

        its 5400 watts

        Comment


        • #5
          Re: dryer element

          from what i have been told , an oven element is made to work in a high heat environment , a dryer element is cooled from fresh air flowing through the element , i know because i have a bunch of elements that come from a central heating system wich is different shape but same type of element. i have been told that they will burn quickly but i did not try them yet