I have a small part that I am sending out to have chromed. I would like to try the Copy Chrome product. It is a small part, steel 4140 about 4 sq inches.
If someone is setup for this, I would like to try a few and the potential will be 100+ per week after.
Yes it does need to be shinny, so buffing is required.
Best regards,
Giles
If someone is setup for this, I would like to try a few and the potential will be 100+ per week after.
Yes it does need to be shinny, so buffing is required.
Best regards,
Giles