    I am looking for someone to plate a few plastic auto interior pieces in a satin/brushed nickel finish. The parts are currently made of plastic so they will need to be coated in silvaspray, then copper plated, then brushed, and finally nickel plated.

    Any one up for the challenge?

  • #2
    I would like to do the job, but Im not sure what kind of finish your looking for. I have done plastic before but it has been a while, so I need to do a dummy piece so I can make sure what I can offer you.
    www.chrome-plater.blogspot.com

    Comment


    • #3
      Yes, also if you have some bondo laying around, I want to make sure that the silvaspray will adhere to the bondo, I don't see why it wouldn't, but I am new to this whole thing


      I can provide you with a photo of the parts needed and finish for a quote. PM me with contact information and we can discuss this further.