Hi,
I'm in Central Florida and have parts I'm manufacturing, but can't find any shops that do production chroming. All of the shops around here want "ungodly" amounts of money to chrome parts due to the Daytona motorcycle scene.
All parts are 6061, T-6, mill finish, aluminm and I can send you dimensioned drawings for review. All parts are either water jet cut or cut on a CNC. All patrs are cut from bar stock, so only the profile has any shape.
The four parts listed below comprise one kit. Part sizes are as follow:
2 at 3/8" x 2" x 12"
1 at 1/4" x 3/4" x 9 1/2"
1 at 1/4" x 3 1/2" x 1 1/2"
I know it's not heavy production but I'd need 5-10 sets done for starters. If all goes well we just get busier.
Thanks,
Jake
I'm in Central Florida and have parts I'm manufacturing, but can't find any shops that do production chroming. All of the shops around here want "ungodly" amounts of money to chrome parts due to the Daytona motorcycle scene.
All parts are 6061, T-6, mill finish, aluminm and I can send you dimensioned drawings for review. All parts are either water jet cut or cut on a CNC. All patrs are cut from bar stock, so only the profile has any shape.
The four parts listed below comprise one kit. Part sizes are as follow:
2 at 3/8" x 2" x 12"
1 at 1/4" x 3/4" x 9 1/2"
1 at 1/4" x 3 1/2" x 1 1/2"
I know it's not heavy production but I'd need 5-10 sets done for starters. If all goes well we just get busier.
Thanks,
Jake
Comment