  • chrome plastic part

    Does anybody have the capacity to do a 29 x 25 x 4 inch deep grille? I would gladly pay to have a plastic part chromed to see what it looks like before making the investment.
    Doug at 3gservices
    734-947-9434

  • #2
    Re: chrome plastic part

    We can handle a part like that, visit www.echromeit.com, Thanks