    Re: Need gloss black Anodize on 3 machined parts

    Misread first post...
    Last edited by ShadowGuy; 08-11-2008, 07:05 PM.

    Leave a comment:


  • busybuildr
    replied
    Re: Need gloss black Anodize on 3 machined parts - DONE

    I want to thank the guys at "Blackcote" for picking up this small work, at a great price, and doing a first rate job with a quick turn-around time.
    You guys are AWESOME !

    Busybuildr

    Leave a comment:


  • busybuildr
    replied
    Re: Need gloss black Anodize on 3 machined parts

    I thank Radmaximus for his response, but the "custom run" cost was a little more than I could afford.

    Anyone out there doing a production run of gloss black, that would be willing to throw these in with the rest of your parts ? I've attached a .pdf drawing, with dimensions, if you're interested.

    [email protected]
    Attached Files

    Leave a comment:


  • radmaximus
    replied
    Re: Need gloss black Anodize on 3 machined parts

    Sent you a PM a couple days ago, check your mail maybe once in awhile.

    Rad

    Leave a comment:


  • busybuildr
    replied
    Re: Need gloss black Anodize on 3 machined parts

    Aw, c'mon ! Nobody wants to do these 3 little pieces for me ? The largest piece is 1.82 diameter x .062 wall, with a .25 flange at one end. The other 2 pieces are similar, but a little smaller.
    I'm looking for a finish similar to a camera lens body (not "gloss", but high sheen ?)
    No polishing required - just clean and coat.
    I would like an experienced finisher who gets consistantly good results, as opposed to someone who is just learning the craft.
    I live in Missouri, but would be willing to ship within the lower 48 if cost isn't too high.

    Any takers ?

    Leave a comment:


  • busybuildr
    started a topic Need gloss black Anodize on 3 machined parts

    Need gloss black Anodize on 3 machined parts

    I have (3) machined tubular shaped parts I need gloss black anodized. These are one-time custom parts, so I'm looking for an experienced anodizer (sorry-no nubies please).

    Anyone interested ?

    I can email pics / dimensions, if needed.

    Thanks,
    Mark