  • Richie95s
    replied to Sealer
    when I add water to my sealer tank due to evaporation, should I add sealer to it as well? Only ran the sealer tank once since it was fresh(about 2 weeks ago) and parts seem to have some smut on them. <br />
    <br />
    To remove the smut, could I dip them in my desmut?
    See more | Go to post

    Leave a comment:


  • Richie95s
    replied to acid bath
    also, when I cleaned my buss har, I used a steel wire wheel to clean it, which I found out later is not a good idea. possibly some fine steel particles may have landed in the bath?
    See more | Go to post

    Leave a comment:


  • Richie95s
    replied to acid bath
    I found a steel bolt in my rack that the customer mistaked as an aluminum bolt. it went through stripper and desmut with other parts. Maybe that caused it? I was out of town last week and I reset my tank with all brand new acid this week. Got it up and running a few racks of parts. I think we're gonna...
    See more | Go to post

    Leave a comment:


  • Richie95s
    replied to acid bath
    after further inspection after I took a few hours to calm myself down, the acid bath is just a bit cloudy. it seems that my last bath setup was a bit more clear. Maybe I'm wrong
    See more | Go to post

    Leave a comment:


  • Richie95s
    started a topic acid bath

    acid bath

    I ran a bunch of parts. All went well. Went out to do a run the next day and I noticed my bath was a bit cloudy and had a brownish tint to it. Any ideas what mightve caused it? It was a fresh bath the same day I ran the first bunch of parts
    See more | Go to post

  • Richie95s
    started a topic Sealer

    Sealer

    I'm using the Caswell Sealer. Instructions say 202°-210°F. I can only get it up to about 180°. Will this be ok if I put run the parts in there longer?
    See more | Go to post
No activity results to display
Show More

Profile Sidebar

Collapse
Profile Picture
Richie95s
New User
Last Activity: 02-02-2018, 02:42 PM
Joined: 02-02-2018
Location:
Working...
X