I've got an electroforming operation plating nickel and cobalt with nickel sulfamate solution and I'm seeing a lot of bubbles/foam forming on top of solution in one of my tanks. Any suggestions on what could be causing it and how to fix?

tank conditions - sparger system pumped from weir...